+86-15123173615

The gasket is a sealing element

Jun 14, 2024

A gasket is a material made of paper, rubber or copper and placed between two planes to strengthen the sealing. It is a sealing element set between static sealing surfaces to prevent fluid leakage.

A gasket is a mechanical seal between two objects, usually used to prevent pressure, corrosion, and natural thermal expansion, contraction, and leakage of pipelines between two objects. Due to the impossibility of perfect machining surfaces, irregularities can be filled with gaskets. Gaskets are usually made of sheet-like materials, such as pad paper, rubber, silicone rubber, metal, cork, felt, chloroprene rubber, nitrile rubber, glass fiber, or plastic polymers (such as polytetrafluoroethylene). Gaskets for specific applications may contain asbestos.

A washer is a loophole (usually in the middle) in a thin plate (usually circular) that is commonly used for distributing load threaded fasteners. Other uses are as spacers, springs (Belleville washers, wave washers), wear-resistant pads, pre display devices, and locking devices. Rubber gaskets are also used in faucets (valves) to cut off flowing liquids or gases. Rubber or silicone gaskets can also be used to reduce fan vibration. Usually, the outer diameter of the gasket is about twice the inner diameter.

 

Material classification

A washer is a component that is placed between a connector and a nut, usually a flat metal ring.

Non metallic gasket is a gasket made of non-metallic materials such as asbestos, rubber, synthetic resin, and polytetrafluoroethylene. A non-metallic jacket gasket is wrapped with a layer of synthetic resin or other non-metallic gaskets.

Semimetallic gaskets are gaskets made of both metal and non-metal materials, such as spiral wound gaskets and metal clad gaskets. A spiral wound gasket is a gasket composed of a V-shaped or W-shaped cross-section of metal tape sandwiched with non-metallic tape, and spirally wound. 1) The inner ring of the inner ring is set on the metal ring of the spiral wound gasket inner ring. 2) The outer ring is set on the metal ring of the spiral wound gasket outer ring. B Metal coating

A metal gasket is a gasket made of metals such as steel, aluminum, copper, nickel, or Monel alloy.

Spiral wound gasket refers to a gasket formed by winding metal tape (usually V-shaped steel tape) and non-metallic tape into a circular shape. The metal tape and non-metallic tape are alternately wound, and due to their good elasticity, they are widely used in flange sealing structures in industries such as petrochemicals, chemicals, and power. Depending on the specific location, steel rings can be added to the inner or outer layer of the gasket to locate or strengthen it.

 

Installation requirements

Installation requirements for gaskets - sealing gaskets

  1. The sealing gasket and flange sealing surface should be cleaned thoroughly, and there should be no scratches, spots or other defects that affect the sealing performance of the connection.
  2. The outer diameter of the sealing gasket should be smaller than the outside of the flange sealing surface, and the inner diameter of the sealing gasket should be slightly larger than the inner diameter of the pipeline. The difference between the two inner diameters is generally twice the thickness of the sealing gasket to ensure that the inner edge of the sealing gasket does not protrude into the container or pipeline after compression, so as not to hinder the flow of fluid in the container or pipeline
  3. The pre tightening force of the sealing gasket should not exceed the design specifications to avoid excessive compression and loss of rebound ability of the sealing gasket
  4. When tightening the sealing gasket, it is best to use a torque wrench. For large bolts and high-strength bolts, it is best to use a hydraulic tensioner. The tightening torque should be calculated based on the given sealing gasket pressure, and the size of the hydraulic pressure of the hydraulic tensioner should also be determined through calculation.
  5. When installing the sealing gasket, the nuts should be tightened in sequence. But it should not be twisted once to reach the design value. Generally, it should be cycled at least 2-3 times to ensure even stress distribution of the sealing gasket.
  6. For pressure vessels and pipelines with flammable and explosive media, safety tools should be used when replacing sealing gaskets to avoid sparks caused by tool contact with flanges or bolts, leading to fire or explosion accidents
  7. If there is a leak in the pipeline, it must be depressurized before replacing or adjusting the installation of sealing gaskets. It is strictly prohibited to operate under pressure

 

Applicable scope

The selection of gasket material mainly depends on the following three factors: temperature, pressure medium

 

Metal gasket material

  1. Carbon steel: It is recommended that the maximum working temperature should not exceed 538 ℃, especially when the medium has oxidizing properties. High quality thin carbon steel plates are also not suitable for use in equipment manufacturing inorganic acids, neutral or acidic salt solutions. If carbon steel is subjected to stress, the equipment accident rate under hot water conditions is very high. Carbon steel gaskets are commonly used for high concentration acid and many alkaline solutions. The Brinell hardness is about 120.
  2. 304 stainless steel 18-8 (chromium 18-20%, nickel 8-10%), recommended maximum working temperature not exceeding 760 ℃. Within the temperature range of -196~538 ℃, stress corrosion and grain boundary corrosion are prone to occur. Brinell hardness 160.
  3. The carbon content of 304L stainless steel shall not exceed 0. 03%. The recommended maximum working temperature should not exceed 760 ℃. The corrosion resistance is similar to 304 stainless steel. The low carbon content reduces the precipitation of carbon from the lattice, and the resistance to grain boundary corrosion is higher than that of 304 stainless steel. The Brinell hardness is about 140.
  4. 316 stainless steel 18-12 (chromium 18%, nickel 12%), with an increase of about 2% molybdenum in 304 stainless steel, improves its strength and corrosion resistance as the temperature increases. When the temperature increases, it has higher creep resistance than other ordinary stainless steels. The recommended maximum working temperature should not exceed 760 ℃. The Brinell hardness is about 160.
  5. The recommended maximum continuous working temperature for 316L stainless steel should not exceed 760 ℃~815 ℃. Compared to 316 stainless steel, it has better stress and grain boundary corrosion resistance with a carbon content not exceeding. The Brinell hardness is about 140.
  6. 20 alloy 45% iron, 24% nickel, 20% chromium, and a small amount of molybdenum and copper. The recommended maximum working temperature should not exceed 760 ℃~815 ℃. Especially suitable for manufacturing equipment resistant to sulfuric acid corrosion, with a Brinell hardness of about 160.
  7. Aluminum (content not less than 99%). Aluminum has excellent corrosion resistance and processing performance, making it suitable for manufacturing double clamp gaskets. The Brinell hardness is about 35. Recommended maximum continuous working temperature not exceeding 426 ℃
  8. The composition of purple copper is close to that of pure copper, and it contains trace amounts of silver to increase its continuous working temperature. The recommended maximum continuous working temperature should not exceed 260 ℃. Brinell hardness is about 80
  9. Brass (copper 66%, zinc 34%) has good corrosion resistance under most operating conditions, but is not suitable for acetic acid, ammonia, salt, and acetylene. The recommended maximum continuous working temperature should not exceed 260 ℃. The Brinell hardness is about 58.
  10. Hastelloy B-2 (26-30% molybdenum, 62% nickel, and 4-6% iron). The recommended maximum working temperature should not exceed 1093 ℃. Has excellent heat resistance and hydrochloric acid corrosion performance. It also has excellent resistance to corrosion from humid hydrogen chloride gas, sulfuric acid, phosphoric acid, and reducing salt solutions. Has high strength under high temperature conditions. The Brinell hardness is about 230.
  11. Hastelloy C-276 16-18% molybdenum, 13-17.5% chromium, 3.7-5.3% tungsten, 4.5-7% iron, all others are nickel. The recommended maximum working temperature should not exceed 1093 ℃. Has excellent corrosion resistance. It has excellent corrosion resistance to various attempts of cold nitric acid or boiling nitric acid with a concentration of 70%, as well as good resistance to hydrochloric acid and sulfuric acid corrosion and excellent stress corrosion resistance. The Brinell hardness is about 210.
  12. Inconel 600 nickel based alloy (77% nickel, 15% chromium, and 7% iron). The recommended maximum working temperature should not exceed 1093 ℃. It has high strength under high temperature conditions and is usually used for equipment that needs to solve stress corrosion problems. Under low temperature conditions, it has excellent co processing performance. The Brinell hardness is about 150.
  13. Monel 400 (copper 30%, nickel recommended maximum continuous working temperature does not exceed 815 ℃. Except for strong oxidizing acids, it has excellent corrosion resistance to most acids and bases. It is prone to stress corrosion cracks in fluoric acid, mercuric chloride, and mercury media, and is therefore not suitable for use in these media. It is widely used in equipment for manufacturing hydrofluoric acid. The Brinell hardness is about 120.
  14. The recommended maximum working temperature for titanium should not exceed 1093 ℃. Under high temperature conditions, it has excellent corrosion resistance. As is well known, it is resistant to chloride ion corrosion and has excellent resistance to nitric acid corrosion over a wide temperature and concentration range. Titanium materials are rarely used in most alkaline solutions and are suitable for oxidation conditions. The Brinell hardness is approximately 216.

 

Non metallic gasket materials

  1. Natural rubber NR has good corrosion resistance to weak acid and alkali, salt and chloride solutions, but poor corrosion resistance to oil and solvents, and is not recommended for use in ozone media. Recommended working temperature -57 ℃~93 ℃.
  2. CR chloroprene rubber is a synthetic rubber that is suitable for corrosion resistance in moderately corrosive acid, alkali, and salt solutions. It has good corrosion resistance to commercial oils and fuels. However, in highly oxidizing acids, aromatic hydrocarbons, and chlorinated hydrocarbons, their corrosion resistance is poor. Recommended working temperature -51 ℃~121 ℃.
  3. NBR nitrile rubber is a synthetic rubber that is suitable for having good corrosion resistance to oil, solvents, aromatic hydrocarbons, alkaline hydrocarbons, petroleum, and natural gas over a wide temperature range. Has good corrosion resistance to hydroxides, salts, and nearly neutral acids. However, in highly oxidizing media, chlorinated hydrocarbons, ketones, and lipids, their corrosion resistance is poor, and the recommended working temperature is 51 ℃~121 ℃.
  4. Fluorine rubber is a mixture of binary and ternary fluororubber fillers and vulcanizing agents. In addition to excellent heat resistance, medium resistance, and good physical and mechanical properties, it also has low compression permanent deformation, good elasticity, and an ultra long service life. Fluorine rubber has outstanding heat resistance (200-250 ℃) and oil resistance, and can be used to manufacture cylinder liner seals, rubber bowls, and rotating lip seals, significantly improving service life. Recommended working temperature: -40 ℃~232 ℃.
  5. Chlorosulfonated polyethylene synthetic rubber exhibits excellent corrosion resistance to acid, alkali, and salt solutions, while being unaffected by climate, light, ozone, and commercial fuels such as diesel and kerosene. But it is not suitable for use with aromatic hydrocarbons, chlorinated hydrocarbons, chromic acid, and nitric acid. Recommended working temperature -45 ℃~135 ℃.
  6. Silicone rubber has outstanding resistance to high and low temperatures, and can be used for an extended period of time at 150 ℃ without any performance changes; It can be used continuously for 10000 hours at 200 ℃ and maintain its unique elasticity, ozone resistance, weather resistance, and other advantages within the working temperature range of -70~260 ℃. It is suitable for making sealing gaskets required in thermal mechanisms, such as sealing rings, valve gaskets, oil seals (suitable for water media), etc. Special silicone rubber can be used to make oil seals.
  7. Ethylene propylene rubber has good corrosion resistance to strong acid, strong alkali, salt, and chloride solutions. But it is not suitable for use in oils, solvents, aromatics, and hydrocarbons. Recommended working temperature -57 ℃~176 ℃.
  8. Graphite is an all graphite material that does not contain resin or inorganic substances, and can be divided into metal doped or metal element free graphite materials. This material can be bonded to manufacture gaskets for pipes with a diameter exceeding 600mm. It has excellent corrosion resistance to many acids, bases, salts, organic compounds, heat transfer solutions, and even high-temperature solutions. It cannot melt, but will sublime when it exceeds 3316 ℃. Under high temperature conditions, caution should be exercised when using this material in highly oxidizing media. In addition to being used for gaskets, this material can also be used to make non-metallic winding tapes in fillers and wound gaskets.
  9. Ceramic fiber and ceramic fiber formed on strips are excellent gasket materials suitable for high temperature and low pressure working conditions, as well as lightweight flange conditions. The recommended working temperature is 1093 ℃, and they can be used to make non-metallic winding tapes in wound gaskets.
  10. PTFE combines the advantages of most plastic gasket materials, including temperature resistance ranging from -95 ℃ to 232 ℃. Except for free fluorine and alkali metals, it has excellent corrosion resistance to chemicals, solvents, hydroxides, and acids. PTFE material can be filled with glass, with the aim of reducing the cold fluidity and creep of PTFE.

Send Inquiry